The machine is made by PWB Interconnect Solutions in Ottawa Canada and the expert is Bill Birch who is heading the IPC Task Group defining tests qualify it. So far it has been correlated to thermal ovens and microsections and at IPC Expo a presentation was made by a staff member form Delco correlating it to the Delco 1000 hour test. Bill may be reached at 819-684-9849 or e mail [log in to unmask] ---------- From: [log in to unmask] To: [log in to unmask] Subject: [TN] Interconnect Stress Test Date: Tuesday, May 19, 1998 5:02PM Has anyone ever heard of an Interconnect Stress Test for bare Printed Wiring Boards? If so, where can I obtain the corresponding coupon in which to perform the testing, as well as how to perform the test? Any help in getting an answer would be gretly appreciated. You can contact me on or off line. Ron Hayashi <[log in to unmask]> ph. # 1-619-695-2222, ext. 243 or Fax me 1-619-695-2165 Thank you very much.. ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################