Hi Darrel Definitely use a star washer or some washer type that will bite through the oxidisation layer. Another option, if you are doing SMT on the boards, is to screen solder paste on the ground plane in a pattern that will contact the bolt head. Have seen this done on a board that needed a good ground path, 150k produced with no ill effects. regards, Graham Collins Process Engineer Litton Systems Canada (902) 873-2000 extension 215 > -----Original Message----- > From: Darrel Therriault [SMTP:[log in to unmask]] > Sent: Wednesday, May 13, 1998 7:22 PM > To: [log in to unmask] > Subject: [TN] OSP and EMI > > Technet, > > My Mechanical Engineers just brought something to my attention that I > would > like to get some opinions/advise/info from the TechNet expertise. > > We have recently switched from HASL to OSP (Entek 106 I believe) finish > for > our boards. We run a ground plane around the perimeter of boards and > backplanes to help with EMI shielding and grounding in general. > > Their concern is with the change to OSP finish, we are seeing bare copper > now that is tarnishing/oxidizing and is this still an acceptable grounding > contact where it bolts to the chassis or contacts a cardcage? > > Other Questions : > > 1. When the board is processed (IR) does the OSP get removed or does it > remain, and > is it conductive or an insulator? > > 2. What are the options for having the ground perimeter copper finished > so it won't > oxidize and will provide a conductive surface for acceptable > ground/EMI contact? > > I would appreciate any comments/opinions/advise. > > Thanks..........DT > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional > information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################