COATES ELECTRA HYSOL LE-RONAL MORTON HAVEN TIAYO ENTHONE GRACE PETERS-GMB are a few that come to my mind On Fri, 1 May 1998 [log in to unmask] wrote > From: Dennis J Fall@TFT on 05/01/98 01:34 PM > > > To: [log in to unmask] > cc: > Subject: Photo imageable solder mask > > Can anyone give me the name of a few companies that manufacture photo > imageable solder mask. Liquid is preferred. Thank You, > > -- > > Dennis Fall > > Thin Film Technology Corporation > > 1980 Commerce Drive > > North Mankato, MN 56003-1702 > > > > Phone: 507-625-8445 x17 > > Fax: 507-625-3523 > > http:\\www.thin-film.com > > mailto:[log in to unmask] > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 > ################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################