Call Shipley, they used to have one. As I recall, there is a lot of difficulty in controlling the tin/lead ratio with an electroless solution, but you can certainly give it a try. In Mpls, call Ken Kamm at 612/476-2794 >>> <[log in to unmask]> 05/06/98 02:31pm >>> From: Dennis J Fall@TFT on 05/06/98 02:31 PM To: [log in to unmask] cc: Subject: Electroless Solder Plating Solution Can anyone give me some info on an electroless solder plating/tinning solution. I know that something has to exist. Thanks ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################