MEK will dissolve alot of plastics but I don't know if it still can be purchased/used. I found Dynaloy in a vender cat list ...see below Dynaloy inc 7 Great Meadows Ln East Hanover NJ Ph 973-887-9270 fax 973-887-3678 Gerry > ---------- > From: RSIMathis[SMTP:[log in to unmask]] > Sent: Tuesday, May 05, 1998 12:47 PM > To: [log in to unmask] > Subject: [TN] Uresolve Plus > > Hi, everyone. > > I'm looking for a chemical (solvent ?) called Uresolve or Uresolve Pls > made by > a company named Dynalloy. (I'm not sure about this name?) This stuff > is used > for dissolving conformalcooatings and potting compounds. Does anyone > have any > information where to purchase this substance OR how to contact this > company? > OR any info about a similar substance? > > What I'm trying to do is dissolve the plastic overmolding on a custom > cable > assembly to check out the internal construction. I'm open to any and > all > suggestions. Thanks for the help. > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for > additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################