Colin, I believe that Gould used to manufacature Ni foil with a treatment for bonding. the Ni foil is still in the MF 150 spec, so someone must still offer it. You could try contacting all the foil vendors. Dave McGowan -----Original Message----- From: Colin <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Date: Thursday, May 28, 1998 6:48 AM Subject: [TN] Nickel foil >Fellow Technetters, > >I have had a request from one of my UK customers, where it would be >possible to source FULLY ANNEALED nickel foil. > >He is looking for 18uM thick foil, treated preferably on both sides, but >one will suffice, in panel sizes around 18" x 12" or 24" x 18". > >Any leads as to where I might get this material, either in Europe or >Stateside? > >Either reply via TechNet, or off-line. > >Thanks in advance. > >Colin McVean >Polyclad Technical Services UK > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. >For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 >################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################