Please send me a copy of the memo> Al Cash fax: 847-870-5746 > ---------- > From: Jim Marsico 516-595-5879[SMTP:[log in to unmask]] > Reply To: TechNet E-Mail Forum.;Jim Marsico 516-595-5879 > Sent: Monday, May 04, 1998 11:26 AM > To: [log in to unmask] > Subject: Re: [TN] flux and stranded wires > > NOTE: THIS IS NOT AN ADVERTISEMENT NOR AN I AFFILIATED WITH ANY FLUX > MANUFACTURERS!!! > > In 1994, as a result of concerns from several military program managers > and > materials engineers, a joint team was formed with the Naval Air Warfare > Center > (China Lake), Hughes Missile Systems (Tuscon, AZ) and Texas Instruments > (Lewisville, TX) to address the issues regarding the use of HF1189 and > HF1189A > water soluble flux on stranded wire. The key issue in this task was to > determine if flux entrapment under the insulation will induce corrosion > and > impact long term reliability. > > On June 15, 1994, a memo was issued from the Deputy Commander for Research > and > Development (Department of the Navy) with the results of the evaluation. > The > results were "None of the data indicates that there will be any problems > with > reliability or performance when stranded wires are soldered with either of > the > subject fluxes." > > The memo is four pages long... the detailed reports from the various > organizations total about 50 pages. I will be happy to FAX the Navy memo > to > whom ever sends me their FAX number, sorry, but the detailed reports are > too > lengthy. > > Jim Marsico > AIL Systems Inc. > (516) 595-5879 > [log in to unmask] > > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional > information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################