A recent thread of messages on TechNet discussed concerns about referencing and obtaining superseded documents and documents with changes in their reference numbers. The governing members of your IPC have tasked the IPC staff to provide the support with obtaining IPC publications that the electronics industry needs. To accomplish this end, Customer Support (under the team leadership of Jean Jones) will make every effort to provide any current or previously published IPC document that is requested. The first effort of Customer Service will be to advise requesters when a revision or change has occurred which now makes the document different than what was originally requested. If the requester is certain that they need/want an older version, Customer Service will coordinate with the appropriate IPC department to provide a copy of the requested document. Note that it MAY only be possible to provide black and white copies of some older color documents. The following information will provide a basic understanding of the numbering changes. For several years your IPC has been involved with IEC, an international (primarily European) standards development association. Once again, based on direction from governing members of IPC, a decision was made to shift FROM IPC UNIQUE document numbering and formatting schemes TO an internationally accepted schemes. This is being phased in based on MAJOR document revisions. As anyone involved with development of standards and specifications is aware, the process is never easy and the bigger the scope, the harder it is to get industry consensus on the whole document. For this reason, when complex documents enter the revision process, they are reviewed to see if they can be broken down into sections to facilitate development and approval. The IPC numbering scheme was merely sequential and the actual numbers usually had no obvious meaning. The international scheme provides four-number blocks in which the first two numbers point to a GENERAL purpose/function. 22nn numbers refer to PWB design. 60nn numbers refer to PWB performance. The last two digits of the block are unique to a "family" of documents with a SPECIFIC purpose/function. The first document in the family will always end in "0". This document will typically be only a few pages and serves the purpose to establish and define that specific family of documents. (This document has no value to the end user, typically will not be published, but can be made available on request.) The primary document in the family will end in "1" and will establish the "generic" requirements that will apply to ALL THE OTHER DOCUMENTS IN THE FAMILY. Examples are IPC-2221 for design requirements for all PWBs, and 6011 for performance requirements for all PWBs. These documents will NOT CONTAIN ANYTHING UNIQUE TO ONLY ONE KIND of PWB. None of this information will be repeated in the other documents so when it is updated, it won't automatically require that other documents be updated also. Other documents in the family will be unique to, in the example above, specific PWBs. IPC-2222 is the design document for Rigid PWBs WHEN USED IN CONJUNCTION WITH IPC-2221. IPC-6011 and IPC-6012 together provide the performance requirements for rigid PWBs. I'm shooting from the hip now because I'm on the road and don't have the documents handy to reference, but I think I remember that IPC-6011 and 6013 are all that a user needs to identify the performance requirements for flex print boards. Other family documents are in development, but the whole effort wasn't held up for the few parts. There is some arbitration on the part of the governing members and Dave Bergman, VP of Technical Programs prior to the decision to renumber documents. For example, IPC-A-600 and IPC-A-610 are in revision and will not be renumbered during this effort; they will only increment one revision letter. The component mounting document IPC-A-770 is becoming IPC-7070 through 7078 (7075 for BGAs, 7078 for Flip-Chip components.) IPC-R-700C became 7711 for Rework of Electronic Assemblies (remove and replace components) and 7721 for Repair and Modification of Printed Boards (laminate, conductors, pads and plated through hole repair/mod.) This got longer that I had hoped. If you have any specific questions, please reply to me OFFNET ONLY. Jack Crawford Project Manager, Assembly [log in to unmask] (847) 509-9700 ext. 393 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################