Try Emerson & Cuming Stycast 1265. It is a two part clear epoxy, and it adheres very well to glass, as long as the glass is clean. For technical data, call Emerson & Cuming Specialty Polymers at 1-800-832-4929. Heidi Jones Senior Manufacturing Engineer Honeywell, Defense Avionics Systems 9201 San Mateo NE Albuquerque, NM 87113-2227 (505) 828-5806 FAX (505) 828-5500 email: [log in to unmask] ---------- From: Jean Connick[SMTP:[log in to unmask]] Sent: Thursday, May 14, 1998 6:01 PM To: [log in to unmask] Subject: [TN] Help Can anyone help me locate an Epoxy, RTV or other, that when cured is semi rigid, with an excellent bond strength to glass. (A one part system is preferred). Thanks for any/all your assistance ahead of time Jean Connick Tel: 714-996-1248 x 299 Fax: 714-961-7836 E-Mail: [log in to unmask] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################