Sorry for my earlier mail without subject ------------ Hi We are getting particles in both component holes / via holes on and off and in double sided / multilayer boards. This is observed after pattern plating We use High build copper and Pattern plating. In some holes the particles are severe and reduce the hole size considerably. The problem is occuring very randomly. Has anybody got remedy for this ? Thanks in advance for the help Milind ______________________________________________________ Get Your Private, Free Email at http://www.hotmail.com ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################