Steve, Our solution was to release all external specs through our document control system. This gives us our own part number to reference. We are then locked into a rev of the external spec, say rev a of J-STD-001. When rev b is available, we make sure we are meeting all the requirements in it before we change our internal copy to rev b. We are not working to the latest revision of the external specs until we make the change in our document control system. Remember, ISO requires you to meet all the requirements of a spec and control it, internal or external. We decided to make all external specs that we wanted to say we meet internal specs. This also forces you to review all new revisions for compliance before saying you meet all its changes. Hope this helps. Regards > -----Original Message----- > From: Steve Keith [SMTP:[log in to unmask]] > Sent: Wednesday, May 13, 1998 9:25 AM > To: [log in to unmask] > Subject: [TN] Esd Standard > > Hello - please forgive me if I am breaking any rules sending this. It > is > my first communication through TechNet. My company recently went > through > an ISO9002 pre-assessment, and one of the points I got hit on was not > having a method in place to make sure I have current copies of > externally > generated documents or specifications. > > My response was to try and find a web site that has the latest > information > posted. > > Can anyone tell me if there is a web site where I can obtain the > latest > specification regarding ESD precautions? > > Also, although slightly off-topic, I am looking for the same thing for > the > ISO9000 standard. > > Thank you for any help. > > Steve Keith > Daisy Disc Corporation > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for > additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################