Hi Technetters Thanks for the good discusion about electroless Ni/Au. I have a simple question! Are there someone who knows where I can material about the chemical reactions that occurs in the electroless nickel bath. We are running a bath with the components Ni, Hypo-phosphit, Ammonia and a lead stabilizer. Regards Jacob Ransborg ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################