GuitarBud wrote: > I recently received immersion gold finished boards from a PCB supplier where > some of the edges of the traces were black. The gold was flaking or had a > bubbled appearance in areas as well. > snip--------------------------------------------------------------------------- Sounds like you have substandard plating. If the gold is bubbled, it probably won't pass a tape test. (You might try performing one on the boards. See any IPC board spec or TM650.) There is no reason that properly applied nickel/gold, either electrolytic or ENIG, should exhibit the characteristics mentioned. As stated by other responders, flakes and bubbles indicate poor adhesion of the plating to the substrate. Since nickel doesn't dissolve appreciably during soldering, do you want to solder to nickel that doesn't adhere to the copper? If the gold bubbled from the nickel, you won't be able to form a reliable solder joint to the passivated nickel under the bubbles. The black material sounds like residual tin or tin/lead. If those contaminates are present in quantities that are visible, the intregrity of both the nickel and gold is suspect. As an aside, I've seen electroless nickel seperate under a tape test when a supplier attempted some rework because all of the pads didn't initiate on the first try. When the gold flakes were examined under magnification, the back sides had nickel coloration and there was nickel on the board at the failure sites. In any case, send the boards back. Don Vischulis ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################