Hello Jim, Try "Solder and Soldering" by Manko. It is a good reference book for solders. Hope you find the information you need. Sundeep Nangalia MCNC [log in to unmask] (E-Mail) ************************************************************************* -----Original Message----- From: Jim Marsico 516-595-5879 <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Date: Thursday, April 09, 1998 12:55 PM Subject: [TN] GEN: PHYSICAL PROPERTIES OF SOLDER |Can anyone tell me where I can get a comprehensive list of the physical |properties (i.e. tensile strength, ductility, modulus, etc.) of different |solder alloys? | |Thanks | |Jim Marsico |AIL Systems, Inc. |(516) 595-5879 [log in to unmask] | |################################################################ |TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c |################################################################ |To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: |To subscribe: SUBSCRIBE TechNet <your full name> |To unsubscribe: SIGNOFF TechNet |################################################################ |Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. |For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 |################################################################ | | ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################