Regarding last week's discussion of copper-gold diffusion> Take a look at Mort Antler's paper in Plating, vol 57, p. 615, (1970) for a discussion of the benefits of a nickel barrier layer in stopping this process. Allan Reed Technic Inc. ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################