Hello All I have seen the various posts on this topic with amusement and my opinion will tend to be different and slightly cynical. I too have a very long history with electroplate Gold and Nickel/Gold systems. Initially we used gold as an etch resist. The same Gold was used for edge contact fingers. The finger spec was 100 microinches of gold over copper and it worked very well. Gold was well under $50 an ounce. Gold went up to $100 an ounce. Because of the cost (and because of gold embrittlement of solder joints!) we converted to tin/lead etch resist. We also converted to "vertical tab plating" for fingers using hard gold, which was a brand new process at that time. Also at that time we added Nickel underplate. The Nickel allowed a reduction in gold thickness while maintaining the ability to pass our tests for porosity and mate/unmate durability. The parameters that met our specs at that time were 70 microinches gold over 300 microinches nickel. The reduction in gold and the added plating precision were a real cost saver. This system also worked very well. Gold prices skyrocketed and consistent supply was uncertain. I can recall long term futures contracts at $400 and $800 an ounce. Security guards supervised all gold adds. A weird time indeed. Also vertical tab plating machines had a hard time meeting the 300 microinch min Nickel req. unless the nickel cell was extremely long. So, the new specs became 70 microinches gold over 150 microinches nickel and these also worked very well. Next came the "commoditization" of PC style memory (a.k.a. the SIMM). Due to cost pressures and the redundant SIMM contact design, the "acceptable" level of gold dropped to 30 microinches and we began seeing even lower cost HASL coated fingers and solder mating connectors. How ell these systems work depends on who you ask. I'll stay quiet on this one..... Today we see a variety of metallurgies that basically serve as gold replacements or extenders.......improvements. The moral of my story is: Technical issues aside (and all opinions I've seen on this subject are basically TRUE), for PWB edge card contacts, what has become "acceptable" over time has largely depended on the price of gold, the and the level of reliability of the board-to-connector contact "system", relative to the level of reliability needed for the end product. Phew......enough history for today. Regards Gerry ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################