I am considering adding a dross reducer in my wave solder pot Have any of you used "DROSS-OUT" made by Chemical and Metals Technology? From the literature it sounds pretty good but I'm skeptical of the claims. Any past experiences, good or bad, with this particular product as well as dross reducers in general would be a great help. Thanks !! Paul Starenas SCI Systems - Hookset NH [log in to unmask] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################