Photocircuits has a production line for electroless Palladium where we produce 10K panels per week. Main use is for the automotive industry, in the audio boards acting as both a solderable surface and a switch contact resistance site. If you wish to contact me off line you can reach me at 516 674 1230 Regards. Gerard O'Brien. Sr. Development Engineer. -----Original Message----- From: Josh Moody [SMTP:[log in to unmask]] Sent: Monday, March 02, 1998 11:21 11:05 To: [log in to unmask] Subject: [TN] eless Pd Technetters, I was wodering if anyone out there is currently using Palladium as a surface finish. I am primarily interested in eless Ni/Pd/ Imm Au. I know that Atotech and LeaRonal both offer this chemistry, but who is using (i.e. end users). What applications are they using it for (i.e. wirebond, solder attach, socket attach of ASICs) Have any assembly problems been identified? Thanks in advance. Josh Moody Materials Quality Engineer Hewlett-Packard - Richardson (HPSD) ph# (972) 497-4617 [log in to unmask] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################