Hi Electroless nickel can be used in a beaker. But; 1. Use a new beaker - scratched ones plate out onto the scratches 2. Make up new each time you use it especially if small volumes Most plating suppliers will have an electroless nickel on their books. - Atotec - Lea Ronal - Cannings Have fun Chris ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################