Jack, It has been my experience that the Laminate Suppliers tend to report Dk on the high Side. We have found, that when applying our Classical Impedance model to the Board build that the apparent Dk is lower than the Suppliers literature. We verified this by measuring Dielectric Spacing and Line widths and Transposing the model to back calculate the Dk. We nearly always found the Actual Dk lower. Within some bounds the higher the resin content the lower the Dk, This is because the Glass reinforcement has a Higher Dk. The composite somewhat follows the "Rule of Mixtures". We usually find the Epoxy Dk to be between 4.0 and 4.2. I hope this is some help. Les Connally [log in to unmask] > From: "Olson, Jack C" <[log in to unmask]>, on 3/3/98 9:21 AM: > WARNING: this is a very unexciting question... > > My software does some basic signal integrity analysis, > and I just noticed it defaults the dielectric constant for > regular FR4 to 4.7 > > I was under the impression that most FR4 is at 4.2-4.3 > these days (more resin? thinner cores? can't remember...) > > Even a brief response will be appreciated! > Jack > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with following > text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional > information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > ################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################