Brad, EIA-481-2 spec. for 16mm and 24mm Embossed Carrier Tape says: "The cover tape shall have a total peel strength of 0.1N to 1.3N (10 to 130 grams calibrated scale reading) for 16mm & 24 mm wide carrier tape. The direction of pull shall be opposite the direction of carrier tape travel such that the cover tape makes an angle of between 165 degrees and 180 degrees with the top of the carrier tape. The carrier and/or cover tape shall be pulled with a velocity of 300 +/- 10 mm/minute during peeling." I do not have any first hand experience with Philips machines, but I recall a local company (Pulsecom) having problems peeling tapes on their Philips machine and they got around it by hanging weights on the take-up reels. Contact me off-line if you would like to talk to someone at Pulsecom and I'll get you a contact in their Mfg Eng group. Steve At 03:13 PM 3/24/98 -0400, Brad Kendall wrote: >I have a major problem with cover tape not peeling off on two part numbers >(16mm tape parts.) At first we suspected the feeders were not working >properly. But all the other 16mm feeders are peeling the parts fine. So >we swapped feeders on those two parts with feeders that were running fine >on the other parts. The problem follows the part, indicating the feeders >are OK. Both parts are from the same vendor and plant, but we are running >other 16mm parts from the same vendor and same plant that work fine. We >have sent back a suspect reel and the vendor peel force tested it and it >falls within their specification. They say they hold a tighter spec. then >the EIA spec. for the part. The peel force as measure by the vendor was in >the range of 72-100 grams. The feeders are supposed to be able to peel >between 900grams and 1Kgram max. > >We have actually had the cover tape rip and break before it peels off! >This again is an indication the peel force is too high on the reel. > >First off, can anyone tell me what the peel force spec is per EIA 481? I >do not have this spec in house. I know one solution is to change vendors. >We seem to be at a standoff with the component vendor blaming the feeder, >but the feeder manufacturer and us saying it is not the feeder as they work >fine on other parts. These reels are NOT PSA tape bonded, they are a heat >seal. One interesting note: the data collected by the vendor during the >packaging process showed peel force of 68-85 grams, but the peel force on >that same reel 3 months later was 72-100 grams. With no adhesive, just a >heat seal process, should that bond get stronger? > >FYI- The parts are Philips Electronics devices and the feeders are Philips >FCM feeders. > >Any suggestions would be greatly appreciated. When the tape does not peel >it not only cost a few parts, but stops a high speed line, that is more >costly then the devices themselves. > >Thanks, >Brad Kendall >Hella Electronics > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. >For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 >################################################################ > > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################