Yes Paul, any information about this test would help. >>> Paul Klasek <[log in to unmask]> 03/17/98 08:40pm >>> Arlene , a lot us ; guys from HP likely most ; but you are a bit laconic to be able to answer . a) of what ? b) thermal cycling on accelerated test ? c) to what standard ? We do here IPC-SM-785 , on flash gold . Let us know . Thanks Paul Klasek ; ResMed >---------- >From: Arlene Infante[SMTP:[log in to unmask]] >Sent: Wednesday, 18 March 1998 9:38 >To: [log in to unmask] >Subject: [TN] Immersion Gold > >Does anyone has an experience/idea on PCB Reliability testing with >Immersion Gold Surface finished? > >a) Temperature? >b) How long on Thermotron chambers? >c) What is the result? > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following >text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional >information. >For the technical support contact Dmitriy Sklyar at [log in to unmask] or >847-509-9700 ext.311 >################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################