Hi all. I have a problem with our Fuji CP642 being able to cut TI carrier tape. The problem is this: > "TI's carrier tape is able to cut into single pieces by Fuji CP642 but > TI's tensile strength is too high. It is 5.3-5.6kg/mm^2 compared to > 2.9-3.3kg/mm^2 of the others. This physical characteristic allows > these single cut-carrier tape to sit on top of each other while it > does not happen with the other vendors. Thus the TI stacked > cut-carrier-tape are too big and heavy for the air vacuum unit of the > CP642 (which was designed to deal with single and equal or less then > 32mm cut-carrier tape only)." > Is there anyone else out there with a CP642 having a similar problem with TI's carrier tape, and if so what have you done to resolve this problem? All comments and suggestions will be greatly appreciated, and thanks in advance! Kathy Palumbo ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################