The IPC-HDBK-001 that Jim refers to below is at the printers, and a formal announcement of its availablility will be made in a few weeks. Please be patient just a bit longer. Jack Jack Crawford, IPC Project Manger - Assembly 2215 Sanders Road, Northbrook IL 60062-6135 [log in to unmask] http://www.ipc.org 847-509-9700 x 393 fax 847-509-9798 >>> "Maguire, James F" <[log in to unmask]> 03/25/98 08:15PM >>> I think the discussion we had in the J-STD-001 Handbook on this subject does a good job of capturing the intent of this section: 8.1.3 Post-Soldering Cleaning (Requirement from 001b) WHEN CLEANING IS REQUIRED, FLUX RESIDUE SHALL BE REMOVED AS SOON AS POSSIBLE, PREFERABLY WITHIN ONE HOUR AFTER SOLDERING. SOME FLUXES OR PROCESSES MAY REQUIRE MORE IMMEDIATE ACTION TO FACILITATE ADEQUATE REMOVAL. MECHANICAL MEANS SUCH AS AGITATION, SPRAYING, BRUSHING, ETC., OR VAPOR DEGREASING AND OTHER METHODS OF APPLICATION MAY BE USED IN CONJUNCTION WITH THE CLEANING MEDIUM. THE TIME BETWEEN SOLDERING AND COMPLETION OF CLEANING MAY BE EXTENDED FOR HAND SOLDERING OPERATIONS, PROVIDED INTERIM CLEANING IS PERFORMED AND COMPLETE CLEANING IS PERFORMED PRIOR TO THE END OF THE PRODUCTION SHIFT. (Rationale) Historically, if a high solids rosin flux is not cleaned from a printed wiring assembly within one hour of mass soldering, the rosin will polymerize, making it nearly impossible to remove or dissolve without destroying the assembly. This can be true to some extent in modern fluxes, as well, hence the one-hour reference. Highly aggressive fluxes, due to their acidic nature, need to be removed more rapidly to limit the attack of metallic surfaces. The method of cleaning solution delivery, or other mechanical aids to cleaning, is left up to the manufacturer. Due to typical logistics of assembly, it may be difficult to do all the hand soldering operations and clean within an hour. Typically, the hand soldering cored wire fluxes are not as immediately harmful (as the wave solder fluxes), so a longer period is allowed, but some measures must be taken to limit the harmful effects of the flux. An example is isopropanol cleaning of RMA fluxes during hand solder, with a more global cleaning by the end of the production shift. The sooner the time to cleaning, the better. Overall, I believe the idea in the 001B wording was (sorry to disagree with Mel) with the extent of cleaning of the PWA. In other words, if you figure to meet your end item requirement for cleanliness for a flux you have to do IPA bench cleaning followed by batch aqueous (not unusual for traditional high solid RMAs to meet environmental/SIR type testing); then you were to complete all the steps necessary to achieve this cleanliness level on the same shift. It should be noted that for technolgies such as SMT, no clean, etc. it has been well documented that simply passing a Resistance of Solvent Extract (ROSE) test (e.g. Omegameter) is NOT an adequate measure of the "cleanliness" of the assembly. ROSE was meant as a process control method (Doug Pauls can go into MUCH more detail on this if you like). The reason was that many of us have had the experience of the "2nd shift guy forgot", "I was out sick and they didn't clean them" or "the planning wasn't updated" when we "string out" the required steps across mulitple days/shifts in the factory. Is bench cleaning "good enough", well if it meets your end item cleanliness level (however you measure/determine it) then yes it is. As an example though, we find that for SMDs hand soldered with RMAs, we can meet Omegameter (13 micrograms NaCl equivalent/in^2) after just IPA bench cleaning but we fail environmental/SIR testing and so we aren't "done" till we go through a follow-on cleaning. On some newer "low residue" fluxes however, we find that little/no cleaning may be required to reach an acceptable cleanliness level (hence our interest in low residue fluxes). How do you know when is "enough"? Well, the testing methodology shown in Appendix D of the 001B is a good place to start and I would also suggest IPC-RT-467 which details the background / supporting data for this appendix. =============================== Jim Maguire Senior Principal Engineer Boeing Information Space & Defense Systems PO Box 3999 M/S 3W-97 Seattle, WA 98124-2499 Phone (253)657-9063 Fax (253)657-8903 Pager (206)982-3737 Email: [log in to unmask] ================================ > ---------- > From: Kenny Bloomquist[SMTP:[log in to unmask]] > Reply To: TechNet E-Mail Forum.;Kenny Bloomquist > Sent: Wednesday, March 25, 1998 1:03 PM > To: [log in to unmask] > Subject: [TN] Completly Clean > > There has been a great deal of discussion in our company about in > process > cleaning. Paragraph 8.1.3 of ANSI J-STD-001 states that "The time > between > soldering and completion of cleaning may be extended for hand > soldering > operations provided interim cleaning is performed and COMPLETE > CLEANING is > performed prior to the end of the production shift." Where we have > trouble > is whit the term "complete cleaning". Assuming that the assembly will > see > further cleaning processes and cleanliness testing prior to conformal > coating, does that mean good bench cleaning practices and inspection > for > flux residue is good enough or does it required batch or in-line > cleaning? > If it does then how clean is clean? If so does this cleaning require > testing to prove that it is "completely clean"? > > I love stuff like this, it's so green and purple. > > Thanks in advance for all responses. > > Kenny Bloomquist > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for > additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################