Lisa, We have had similar issues with the lack of CEM 3 material. We have convinced our customers to use glass steal products. It has basically the same characteristics as far as the only having glass fabric on the top and bottom of the construction and cost was less. However, It is not paper base. Their number is 901 853-5070. Hope this helps. Ed Cosper ---------- From: Lisa Parker[SMTP:[log in to unmask]] Sent: Friday, February 06, 1998 2:36 PM To: [log in to unmask] Subject: [TN] I need .059 1/1 or 1/0 GE CEM3 or AL910 laminate I need some GE CEM3 .059 1/1 or 1/0 or Norplex Oak AL910 .059 1/1 or 1/0 laminate. The minimum size I can use is 18x24. GE discontinued manufacturing CEM3 around the third quarter of 1997 but I still have customer requirements for GE CEM3. Allied Signal also discontinued manufacturing Norplex Oak AL910 around the first quarter of 1997 but I still have customer requirements for AL910 also. If you or anyone you know has some GE CEM3 .059 1/1, 1/0 or Norplex Oak .059 1/1, 1/0 laminate on hand and would be willing to sell some, please let me know as soon as possible. I can be reached at: phone 316-431-0406 x219 fax 316-431-2013 E-mail: [log in to unmask] Thanks! Lisa Parker Purchasing Agent ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################