Hi Matthew, I can't comment on the brown residue that you're seeing, but we've also noticed OSPs that exceed the so-called "maximum" thickness value. We had a similar situation with the dip tank and the spectrophotometer, yet we had an analytical lab show measurements of up to 3X the max thickness (1.5 microns). I seem to remember that the technique used was some sort of ellipsometric method, but I'm not sure. I believe that the discrepancies between our measured values and the published maximum thickness can be explained when you consider that the latter is based on data from flat, uniform copper coupons, and not on actual boards. Regards, Greg Bartlett Mercury Computer Systems Chelmsford, MA [log in to unmask] Matthew Park wrote: >Entek Plus data spec from Enthone specified a coating >thickness of 0.35um (min 0.2um to 0.5um max). My pcb vendor >follows this thickness req. and performs a UV >spectrophotometer test as per a batch cycle to measure the >coating thickness. (By the way the vendor uses dip-tank process >for coating Entek-Plus) I am seeing brown residues on TH >solder joints (not on smt solder joints after reflow) after >wavesoldering. > >I am drawing a conclusion that the cause of brown residue is as >the result of much thicker coating in plated TH holes. I believe >heat and flux (2% no clean flux) do not have a time to dissolve >and evaporate the coating in plated TH holes. Semi-dissolved >coating in TH holes gets pushed up toward the component side >by molten solder. Thus causing spotty brown residue on TH >solder joints on the component side of boards. > >The reduction of belt speed (3.5ft/min) and some heat increase >do not reduce this residue. Hand-soldering of TH holes were >performed with the same result as per previous e-mail >message. > >I wish I had a damn micrometer to measure that coating >thickness, or Is there more stuff??? > >regards >Matthew Park >NII Norsat International Inc. > >######################################################## >######## >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >######################################################## >######## >To subscribe/unsubscribe, send a message to [log in to unmask] with following >text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >######################################################## >######## >Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional >information. >For the technical support contact Dmitriy Sklyar at [log in to unmask] or >847-509-9700 ext.311 >######################################################## >######## > > > >RFC822 header >----------------------------------- > >Return-Path: <[log in to unmask]> >Received: from charon.mc.com by mc.com (SMI-8.6/SMI-SVR4) > id RAA14442; Tue, 10 Feb 1998 17:56:30 -0500 >Received: from jefry.ipc.org (na-3.megsinet.net [208.150.51.11]) > by charon.mc.com (8.8.8/8.8.8) with ESMTP id RAA08241 > for <[log in to unmask]>; Tue, 10 Feb 1998 17:56:37 -0500 (EST) >Received: from jefry (208.150.51.11) by jefry.ipc.org (LSMTP for Windows NT >v1.1a) with SMTP id <[log in to unmask]>; Tue, 10 Feb 1998 16:44:45 >-0600 >Received: from IPC.ORG by IPC.ORG (LISTSERV-TCP/IP release 1.8c) with spool id > 54584 for [log in to unmask]; Tue, 10 Feb 1998 16:44:40 -0600 >Received: from simon.ipc.org by jefry.ipc.org (LSMTP for Windows NT v1.1a) with > SMTP id <[log in to unmask]>; Tue, 10 Feb 1998 16:44:40 -0600 >Received: from norsat.com by simon.ipc.org via SMTP > (951211.SGI.8.6.12.PATCH1502/940406.SGI) for <[log in to unmask]> id > QAA06490; Tue, 10 Feb 1998 16:50:41 -0800 >Received: from NORSAT-Message_Server by norsat.com with Novell_GroupWise; Tue, > 10 Feb 1998 14:56:12 -0800 >X-Mailer: Novell GroupWise 4.1 >Mime-Version: 1.0 >Content-Type: text/plain >Content-Disposition: inline >Message-ID: <[log in to unmask]> >Date: Tue, 10 Feb 1998 14:55:59 -0800 >Reply-To: "\"TechNet E-Mail Forum.\" <[log in to unmask]>, > Matthew Park" <[log in to unmask]> >Sender: TechNet <[log in to unmask]> >From: Matthew Park <[log in to unmask]> >Subject: [TN] Entek Plus coating thickness >To: [log in to unmask] >X-UIDL: e49882d66e2716dd98e53fe303f14fb9 > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################