Koushik, The crackling noise, at least when the board is in or coming out of the reflow oven, sounds like it could be due to "popcorning" - plastic parts that absorb moisture during storage and which expands during heating in the reflow oven. This results in stress which can cause cracks (the "popcorn" noise) in the package and create other damage which may not be caught at test. Have you closely examined your larger plastic parts on the board for any such damage? Have they been handled prior to reflow according to the appropriate JEDEC moisture sensitivity number for those parts? Steven Lustig Process Engineer EMS Technologies Norcross, GA (770) 263-9200 x4714 [log in to unmask] >---------- >From: Koushik ATD Banerjee[SMTP:[log in to unmask]] >Sent: Thursday, February 26, 1998 2:41 PM >To: [log in to unmask] >Subject: [TN] Question : "Crackling" noise in boards post SMT > >I would like to request for input / feedback on an interesting problem >that we are seeing sporadically in our SMT line. > >Some of the PCBs, post component attach, when they are either in or >are coming out of the reflow oven are making a "crackling" noise ! We >have not identified any defects in the boards or the components yet >and we are unsure what is causing the noise. Sometimes, we are also >hearing this noise when we take a board in our hands post SMT and try >to warp it a little ! The boards are approx 5" x 12", have components >on both sides (passives and some actives) and is not very densely >populated. Any suggestions on what could be the reason would be >greatly appreciated ! > >Thanks,-Koushik Banerjee- > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following >text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional >information. >For the technical support contact Dmitriy Sklyar at [log in to unmask] or >847-509-9700 ext.311 >################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################