We are interested in the impact of a micro via dimple or laser via in BGA pad. General construction would consist of a laser via 3 -5 mil diameter (2 - 4 mil diameter after plating) in a dielectric material 2 - 3 mils thick. I understand that microvia cleanliness is crucial. Any moisture or chemical residue left in the dimple could out gas and produce a void in the solder ball during the assembly process. Is this a reliability issue? Will improved PWB cleaning and packaging methods will be required to keep microvias clean and dry? Do PWB methods exist to minimize the dimple in the PWB? Do assembly clean or paste methods exist to eliminate voids in the solder ball? Thanks for your interest and any response you may have, Dave Backen ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################