-- [ From: Tony Bugeja * EMC.Ver #2.5.02 ] -- Is it a big problem running gold connectors in your wave solder? Will it contaminate your pot? Or is this just a myth? Doesn't alot of the gold just end up being dross? -- Tony Bugeja, P.Eng. E-Mail: [log in to unmask] Process Engineer Phone: (204) 631-7241 C-Mac Electronics Fax: (204) 631-7294 1455 Mountain Ave Wpg., Mb. R2X 2Y9 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################