>Dear Technetters, > >I have seen the most weird problem in my 7 years in PCBA manufacturing >environment. Solder is getting between the epoxy and component and/or >between fab and epoxy thus shorting it out across terminations of SMT caps. > >Does any one has seen similar problem? Any resolution? Our regular process >is epoxy application thr' stencil, component loading, curing and then hand >load & wave. > >Any help or leads will be highly appreciated. > >re, >ken patel Ken, Check moisture absorption of the PWB to see if it is out gassing during cure causing bubbled to form underneath the chip. Also check the cure schedule to insure that it does not exceed the maximum temperature. Some materials can out gass under excess cure conditions. John Maxwell ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################