Jim, And I suppose you want it to be cheap, readily available, low toxicity, ozone friendly and not a global warmer, right? And people wonder why we chemists go a bit strange! People want alchemists.I I would say Axarel 2200 is as close as I have seen on the market so far. I am expecting that we will see some very good things with n-propyl bromide in the very near future. regards, Bev Christian Nortel > ---------- > From: Jim Marsico 516-595-5879[SMTP:[log in to unmask]] > Sent: Monday, February 23, 1998 11:50 AM > To: [log in to unmask] > Subject: [TN] ASSY: HAND CLEANING > > Has anyone found a cleaning solution for hand cleaning (bench top) > operations > which is nonflammable, pleasantly smelling, quick drying and > adequately cleans > rosin flux residue? If so, please send me information on this miracle > solvent. > > Thanks, > > Jim Marsico > [log in to unmask] > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for > additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > ################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################