Steve, From about 13 years of TH only Automated Insertion experience, we have always used .014" over nominal. We based this on the equipment we bought, that being Universal Instruments, and the fact that we were not smart enough to look at IPC standards, or any other for that matter, to find an industry standard. It has worked very well for us for these years. Based on the info you presented here, we seem to be on the low side of things. However we do not seem to be any less for the wear as it were. Hope this helps in some way. Richard Hamilton Clemar Mfg. / Rain Bird [log in to unmask] > -----Original Message----- > From: Steve Collins [SMTP:[log in to unmask]] > Sent: Monday, February 23, 1998 11:22 AM > To: [log in to unmask] > Subject: [TN] DES: Hole sizes for non-auto-insertable parts > > Technetters: > > I have been using the IPC guidelines for Radial & Axial part hole > sizes for > some time now for non-auto-insertable parts. I was doing this because > from > my way of thinking all parts are either radial or axial just not all > are > auto-insertable. My question is, if I'm working to IPC-D-275 level B > is it > safe to split the dimensions shown in table 5-15. What I mean is this > table > calls out for "No greater than 0.7 mm (0.028) over minimum lead > diameter" > and " No less than 0.20 mm (0.008) over maximum lead diameter." Since > there > is a .020 difference from min to max I would like to split this and > use > .010 plus the min .008 for .018 over nominal lead diameter for these > types > of parts. Does this thinking justify itself for most applications. > > Steve Collins > Antec Corporation > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################