We are having problems with the new XZ17B catalyst from Coates When we try to use it the ink bleeds over onto the pads during stoving. We have been using the old XZ17T for 15-20 years and never had any problems. So far Coates Technical support has to date failed to come up with any useful advice. Has anyone any recommendations for a ink we could change onto or any ideas relating to our problem ? -- Roger Unwin http://www.p-m-services.demon.co.uk ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################