I need some GE CEM3 .059 1/1 or 1/0 or Norplex Oak AL910 .059 1/1 or 1/0 laminate. The minimum size I can use is 18x24. GE discontinued manufacturing CEM3 around the third quarter of 1997 but I still have customer requirements for GE CEM3. Allied Signal also discontinued manufacturing Norplex Oak AL910 around the first quarter of 1997 but I still have customer requirements for AL910 also. If you or anyone you know has some GE CEM3 .059 1/1, 1/0 or Norplex Oak .059 1/1, 1/0 laminate on hand and would be willing to sell some, please let me know as soon as possible. I can be reached at: phone 316-431-0406 x219 fax 316-431-2013 E-mail: [log in to unmask] Thanks! Lisa Parker Purchasing Agent ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################