We are using glue printing on solder side for cases where there are no tht parts.We have used glue print quite a bit. However, we are still in search for a good method to print glue on mixed technology assemblies where clinched leads demands clearance of order of 45-60 thou of inch. Currently, I am working with one company to work out engg stencil for one mixed tech assy. Any technet expert on this can advise me .Of my own, I might have to do expensive trials before I can reach the solution- Please post your advise on technet. ashok > ---------- > From: Peggi J. Blakley[SMTP:[log in to unmask]] > Sent: February 24, 1998 7:54 AM > To: [log in to unmask] > Subject: Re: [TN] Glue dispenser machine v/s stencil printing > > Are you the Ken Patel that use to work for Honeywell in San Diego many > moons > ago? > > At 07:03 PM 2/23/98 -0800, you wrote: > >Can anyone tell me what Motorola is using to dispense the glue > (epoxy)on > >solder side, glue dispenser or trough stencil printing? Does anyone > know any > >contact house uses glue printing method? > > > >Any help will be appreciated. > > > >re, > >ken patel > >______________________________________________________ > >Ken Patel Phone: (408) 490-6804 > >1708 McCarthy Blvd. Fax: (408) 490-6859 > >Milpitas, CA 95035 Beeper: (888) 769-1808 > > > >################################################################ > >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > >################################################################ > >To subscribe/unsubscribe, send a message to [log in to unmask] with > following > text in the body: > >To subscribe: SUBSCRIBE TechNet <your full name> > >To unsubscribe: SIGNOFF TechNet > >################################################################ > >Please visit IPC web site (http://jefry.ipc.org/forum.htm) for > additional > information. > >For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > >################################################################ > > > > > Peggi J. Blakley > NAVSURFWARCENDIV Crane > Code 7062, Building 3241 > 300 Hwy 361 > Crane, In 47522-5001 > Voice: 812-854-2086 > Fax: 812-854-3855 > DSN: 482-2086 > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for > additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################