Chris First you should be aware that the soon to be released revision of the IPC-CC-830 will EXCLUDE adhesion testing. Why? Because there seems to be no correlation between adhesion of the Conformal coating with circuit reliability. Remember that the coating is tested independently onto bare coupons (as are all other surface coatings: resists, fluxes pastes etc) and adhesion in this condition has not seemed to be an issue. However, when you put a resist in between and adhesion sometimes seems poor? - The coating is not intelligent - so how does it know any difference?? Also, are you using a silicone coating? If so, how is any tape (used in such adhesion tests in the past) going to stick to the coating to make the test meaningful? Have you experienced a reliability problem? Are you testing the coating for failure? Please advise.... Regards, Graham Naisbitt __________________________________________________________________________ [log in to unmask] Concoat Ltd Alasan House, Albany Park Camberley GU15 2PL UK http://www.concoat.co.uk -----Original Message----- From: Chris_Smith <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Date: 12 February 1998 19:59 Subject: [TN] Conformal Coat adhesion testing? > All, > I am currently seeking a place to purchase a roll of mesh to do > conformal coat adhesion testing with. What I've found so far is that > it should have 1/8 inch squares and should be an 1in wide. It will be > made of a fiberglass, Holland cloth or a Dacron cloth material. If > anyone has any other information or areas I could look please let me > know. > > Thank you > Chris Smith > Manufacturing Eng. > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. >For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 >################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################