Hello All: I need help trying to minimize "organic" contamination occuring in a cupric chloride final etch. The contamination is a "black", gummy material which floats on the surface of the bath in clumps. If the line is not cleaned periodically, black spots on the surface of copper (typically not the laminate), can be seen in inspection. The DES line processes only innerlayers utilizing CibaGiegy (0.9 mil nominal thickness) and Dyanchem FL 1.3 mil photopolymers as etch resists. An FTIR scan has been performed on the residue, both photopolymers, and the "rollers". While not entirely conclusive, the scans more closely resembled the photopolymers and not the rollers. Visually, the rollers do not seem to be swelling or deteriorating. The etching bath is operated at 1.3 N HCl, regenerated via chlorine gas (ORP control), and sees both 1 oz and 2 oz copper. I am unsure of the laminate being employed. Continuous carbon filtration has been employed with some degree of success. The carbon filters are changed weekly: one 30" filter per 450 gallons of bath. Can anyone offer suggestions to better control or eliminate this residue?! Thanks in advance Ted Stern ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################