Item # 1 is, indeed, legit. Item #2 is also since "fresh" etchant, w/o Cu will not etch, so the etchant that is rinsed from the exiting panels does increase the Cu content. Item #3 is propaganda. Al Hamilton ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################