We are also using a UV cure adhesive. Dymax sells a two pedal system which lets you apply the adhesive by air-syringe and then the other side of the pedal operates the fiberoptic light to cure it, all mounted in one wand. There are many different adhesives to pick from, but the properties in Jims' email below are desirable. Faster cure times are possible depending on the bondline and application. This seems to be the best way to connect teflon type insulations to FR4, as TakPaK will lift during thermal cycling . At 12:49 PM -0400 1/12/98, Jim Marsico 516-595-5879 wrote: >Try a UV curable adhesive. We're using a Masterbond product UV15-7TK1A. >It is >a one-part epoxy which cures in about 30 seconds when subjected to a UV light. >It is low-flow (it stays where you put it), solvent resistant, and can be >removed after cure, if necessary. Phillip A. Bavaro Senior Manufacturing Engineer [log in to unmask] (619) 658-2542 ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################