The IPC limit for contamination is 10.07 ug / sq in NaCl equiv. The 3 ug limit is good for no-clean, but naturally the cleaner the better. >>> Ken Patel <[log in to unmask]> 01/26/98 05:25pm >>> Allan, Can you or some one clarify... If the board is more than 3 mg. cl. sq. in.in terns of contamination, PCBs are reject for no clean assembly process. Is it mentioned somewhere in IPC and also what is the limit for those PCBs going through regular water soluble paste and flux chemistry? re, ken patel At 05:16 PM 1/23/98 -0500, Allan Kerr wrote: >HASL does not leave a flat surface for the screen print operation, this is >especially true for very fine pinch boards. Plus OSP is a "cleaner" >process, MANY of the fab shops are not properly equipped to clean >boards after the HASL operation. If a fab shop can't clean a board to <3 >mg. cl. sq. in. they shouldn't sell boards that are to be used in a no-clean >process. I'm sure CSL will add to this one. This is a BIG issue to all of us >building high reliability products. > >>>> Sheila Smith <[log in to unmask]> 01/23/98 03:27pm >>> >Hello, Please refresh my memory ... what are the >advantages/disadvantages >of HASL over other processes? Specifically, why would a Customer >direct a >PWB supplier that HASL is not to be used ...? > >Sheila Smith > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV >1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with >following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional >information. >For the technical support contact Dmitriy Sklyar at [log in to unmask] or >847-509-9700 ext.311 >################################################################ > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. >For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 >################################################################ > > > ______________________________________________________ Ken Patel Phone: (408) 490-6804 575 Cottonwood Dr. Fax: (408) 490-6859 Milpitas, CA 95035 Beeper: (888) 769-1808 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################