Mark, Given that all fluxes leave residues, the issue is how will they inter-react with the other process chemistries you have on your assembly. In addition, we know that the higher the operating frequency, the more the electrons migrate to the periphery of the conductor so, where they interface with the board surface, you will have an area of high potential for electro-chemical reactions. Are you able to predict these and verify that they will not be harmful to long term reliability? SIR testing developments will permit you to do this by measuring the amount of leakage that is occurring. Use a voltage gradient of 100v/mm that will better mimic your assembly operating conditions, apply frequent monitoring so that you do not miss any dendrite formations (electro-chemical migration) and use current limiting resistors to preserve them for further analysis. Bear in mind that dendrites are known to form within 20 minutes under the right conditions. You should then be better placed to determine the reliability of your assembly. I hope this helps - let me know if you would like more Graham Naisbitt __________________________________________________________________________ [log in to unmask] Concoat Ltd Alasan House, Albany Park Camberley GU15 2PL UK http://www.concoat.co.uk Application Engineers in Chemical Compounds to the Electronics Industry -----Original Message----- From: [log in to unmask] <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Date: 21 January 1998 14:22 Subject: [TN] RF Circuitry and Rosin Core Solder > Hello All, > > Has anyone dealt with or have found any issues with using a Rosin Core wire > solder on RF circuitry? Like Kester (no clean) "282" Rosin Core (63/37) > We have heard of "theories" that the flux left behind after soldering > has some negative effect on the operation of the RF Circuit. Anyone? > > Thanks, > > Mark Pozorski > ADC Telecommunications > >############################################################## >TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c >############################################################## >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TECHNET <your full name> >To unsubscribe: SIGNOFF TECHNET >############################################################## >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. >For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 >############################################################## > ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################