Fred, The company which I work for is just started to changeover to no-clean. From the trials which we have carried out to date the best general all round flux has been Alpha SLS 65. We have been successful in achieving reflow on 90 thou boards using an Econo-Pack spray fluxer and an air knife on an Electrovert UPK 600. However the PCB's which we are building are not densely populated with thru-hole components. Martin Bourke. ---------- > From: [log in to unmask] > To: [log in to unmask] > Subject: [TN] Any No Clean Flux for Thick PCB's? > Date: Monday, January 05, 1998 10:54 AM > > Has anyone had any success using a no-clean flux on thick (0.090") multi-layered > thru-hole PCB assemblies? > > We want to switch to a no-clean flux from our present aqueous system. Our > Electovert currently has a foam fluxer but would get a jet-sprayer if the flux > was right. However, we tried a few demo no-clean fluxes and experienced problems > with our larger and thicker multilayer boards as far as solder wicking up to the > top-side on feed-thru's. We even added extra heated air-knives and to no avail. > > If you have had success with any particular no-clean fluxes, please let me know > what they are. > > Thank you. > Fred > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################