Jacob, You may be unwise to apply a coating of any description to aged assemblies. Please consider that coatings seal in as well as out. You say that the corrosion is worse after repair which would be consistent with flux residues left behind. Are you able to clean the re-worked area effectively? You might want to try some of the new aerosol cleaning materials such as those from TechSpray Inc Chemtronics(?) or perhaps Electrolube, at least they will help to reduce the amount of residue. Alternatively, why not try a no-clean low residue solder, that may help. If you do use a coating, then an Acrylic would be ideal as it's easy to use, fast to cure and solderable. Graham Naisbitt __________________________________________________________________________ [log in to unmask] Concoat Ltd Alasan House, Albany Park Camberley GU15 2PL UK http://www.concoat.co.uk Application Engineers in Chemical Compounds to the Electronics Industry -----Original Message----- From: Jacob Mozel <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Date: 28 January 1998 12:45 Subject: [TN] Conformal coating >Hi TechNet, > >I'm working for a big repair lab of cellular phones. For a long time we >experience returning of many cellular phones due to corrosion, specially >after repairing. >I thought about using a conformal coating to protect the fresh solder >from humidity and moisture. >Does anyone has got an experience in this kind of work and could >recommend easily removable coating (we do not seek solvent protection), >the application method and curing mode (since there are expected many >shaded points, UV or any radiation curing does not seem feasible). > > >Thanks > >Jacob Mozel > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. >For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 >################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################