MOST SMT COMPONENTS ARE PLASTIC PACKAGES . I HAD EXPERIENCED REMOVAL OF COMPONENT MARKING ONCE THE COMPONENTS ARE EXPOSED TO ACETONE AT 40-50 DEG C EVEN FOR SHORT DURATIONS. ACETONE IS CORROSIVE EVEN TO SS. IT MIGHT AFFECT RELIABILITY(CORROSION) AS PLASTIC PACKAGES MIGHT ABSORB SOLVENT . > ---------- > From: Chan, Marcelo[SMTP:[log in to unmask]] > Sent: January 27, 1998 2:39 PM > To: [log in to unmask] > Subject: [TN] Acetone of SMT assemblies > > What are the drawbacks to using Acetone as a solvent on a fully > assembled PWB with surface mount components? The idea is to dip the > entire assembly for about 15 minutes....Would the epoxy molding on > components absorb the acetone? What about the soldermask? > > Marcelo > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for > additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################