Sam, are the dishdowns everywhere on the circuits, or are they located where there are holes only. There are a couple of things you may want to look at: 1) Check your developer, make sure the boards are getting a good rinse. 2) If the "dishdowns" are on the circuits only. Check to see if they are located on both sides of the boards. If only on one side, is it the side that the circuits would be horizontal in the plating tank? If so, check your sparging system, you may be experiencing microbubbles attaching to the circuits during pattern plating. ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################