IPC announces the availability of IPC-CF-152B, Composite Metallic Material Specification for Printed Wiring Boards. IPC-CF-152B addresses the requirements for copper/invar/copper, copper/molybdenum/copper composites used in electronic applications. At the end of the document is a series of spreadsheets, which outline engineering and performance data for composite materials. The specification sheets are provided with a number for ordering purposes. Chair: Rolland Savage, Gould Electronics, Inc. members $15 nonmembers $30 IPC-CF-152B is available through the IPC: phone: 847-509-9700 fax: 847-509-9798 e-mail: [log in to unmask] URL: www.ipc.org ################################################################ IPC_New_Releases E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE IPC_New_Releases <your full name> To unsubscribe: SIGNOFF IPC_New_Releases ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################