IPC announces the availability of IPC-4101, Laminate/Prepreg Materials Standard for Printed Boards. IPC-4101 covers the requirements for base materials (laminates or prepregs) to be used primarily for rigid or multilayer printed boards for electrical and electronic assemblies. At the end of the document is a series of specification sheets, which outline requirements for both laminate and prepreg by product grade. The specification sheets are organized by specific reinforcement type, resin system, and/or construction and are provided with a Specification Sheet Number for ordering purposes. IPC-4101 supersedes IPC-L-108, IPC-L-109, IPC-L-112, IPC-L-115, and IPC-AM-361. Chair: Erik Bergum, Polyclad Laminates, Inc. members $40 nonmembers $80 IPC-4101 is available through the IPC: phone: 847-509-9700 fax: 847-509-9798 e-mail: [log in to unmask] URL: www.ipc.org ################################################################ IPC_New_Releases E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE IPC_New_Releases <your full name> To unsubscribe: SIGNOFF IPC_New_Releases ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################