Thanks for the information Tomer Paul Gould wrote: > Tomer wrote:- > >1) We are interested in tape as protection for gold connectors > before > >HAL. > >2) We are looking for special rubber (If there is such) to clean > "dark > >gold fingers" > > 1)We use a red paper tape FOUR PILLARS? (I think!) CM8R. It withstands > > HASL very well and peels with no adhesive transfer so no cleaning > necessary. A simple tape dispenser can be used or an automatic pre- > cutting machine if the areas are isolated and length critical. > > 2)If you want to polish up tarnished gold then an ordinary ink rubber > should be sufficient. They are not too abrasive. I would suggest that > the contacts should not need to be cleaned in this way and this > usually > indicates a problem with the gold plating. > > Regards > Paul Gould > [log in to unmask] > Isle of Wight,UK > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV > 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or > 847-509-9700 ext.311 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################