The October Project Section of ITRI is surveying the industry for techniques of filling both conductive and non-conductive materials into vias. The final objective is design of a challenging multilayer microvia test structure. However, a subcommttee is surveying the fill of both conventional through board vias and filling microvias for planarization. Planariztion is critical to make multilayer microvias, particularly with the vias vertically stacked for maximum density. Committee work underway includes literature and patent searches, process descriptions, and this TechNet survey to see the state of technology. John Davignon of Merix is the overall Task Group Chairman, and Rich Wessel of DuPont is section chairman on via filling. I just boasted that TechNet would be a good source of information to meet our survey deadline of January 9, so I get to send this. How are you filling vias today in your shop? Denny Fritz MacDermid - Waterbury ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################