I would appreciate hearing from or about a contract repair shop that is equiped to perform PBGA replacements. We are located in Carson City, Nevada so we would prefer a California or Nevada shop. The boards are a small quanitity of 7"x13", 8 layer, FR, utilizing the Intel FW82439HX PBGA chip. Problem has been isolated to opens under the BGA. Replacement ICs are provided. Lee McCuistion Manufacturing Engineer Cubix Corporation 2800 Lockheed Way Carson City, NV 89706 702-888-1000 x237 (voice) 702-888-1002 (fax) [log in to unmask] (e-mail) ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ##############################################################